Main features >> Technical data
Technical data
| TEMPERATURE RESISTENCE | |
| Operating temperature (ºC) | From -40 to +180 |
| Coefficient of linear expansion (mm/mK) | 0,025 |
| LIGHTNESS | |
| PPSU vs COPPER / BRASS | 7 times lighter |
| PPSU vs PPR | |
| LOW INTERNAL ROUGHNESS | |
| Pressure drop | Lower than any other traditional system |
| INNOCUOUS MATERIAL | |
| Oxide migration to water | 0 |
| Production of harmful substances in water | 0 |
| THERMAL INSULATION | |
| Thermal conductivity (W/mK) | 0,35 |
| PPSU vs BRASS | 400 times less |
| PPSU vs COPPER | 1400 times less |
| ELONGATION BY BREAKING | |
| Elongation by breaking (%) | From 60 to 120 |
| RESISTANCE AGAINST CHEMICAL AND OXIDANT AGENTS | |
| Suitable for drinking water | Yes |
| Suitable for industrial applications | Yes |
| Resistance against chemical agents | Stable |
| Compatible with usual constructive materials | Yes |
| Performance with low Ph water | Stable |
| ACUSTIC INSULATION | |
| Silent water flow | Yes |
| CERTIFICATES | |
| Spain (AENOR) | UNE EN ISO 15875 |
| Portugal (LNEC) | DH 888 Certificate |
| REPRESENTATIVE TESTS | |
| Thermal cycling test | 5.000 cycles, from 95 ºC to 20 ºC, 10 bar |
| Pressure cycling test | 10.000 cycles, from 12 bar to 0,5 bar, 23 ºC |
| Internal pressure test, 95 ºC | From 8,82 bar to 16 bar; from 1 hour to 1000 hours |
| Internal pressure test, 20 ºC | From 23,92 bar to 40 bar; 1 hour |
| Vacuum watertightness test | 0,8 bar, 1 hour, 23 ºC. Result: No pressure variation. |
| Elongation by breaking, 95 ºC | 181 N, 1 hour, 95 ºC. Result: It stands. |
| Elongation by breaking, 23 ºC | 121 N, 1 hour, 23 ºC. Result: It stands. |
Available news
01/09/20108 - 11 September 2010. INTERBUILD AFRICA 2010.
Untitled document Show dates:...
02/09/201015 - 19 March 2011. ISH FRANKFURT. Germany
Untitled document PLOMYPLAS G...
02/09/201020 - 23 October 2010. AQUA-THERM. BAKU. Azerbaijan
Untitled document PLOMYPLAS...
02/09/201027 - 30 September 2010. INTERBUILD JORDAN.
Untitled document PLOMYPLAS G...